Skip to Content
Fern + Roe
About
About Hide Tanning
Hide Tanning Resources
Hide Tanning Tips
Fern + Roe FAQs
Learn With Us
Courses we offer
Upcoming In-person Courses
Private Group Instruction
Hide Club
Self-paced online courses
1:1 Mentorship
Hide Club: SUMMER CAMP
Shop For Tools
0
0
Visit Upcoming Courses
Fern + Roe
About
About Hide Tanning
Hide Tanning Resources
Hide Tanning Tips
Fern + Roe FAQs
Learn With Us
Courses we offer
Upcoming In-person Courses
Private Group Instruction
Hide Club
Self-paced online courses
1:1 Mentorship
Hide Club: SUMMER CAMP
Shop For Tools
0
0
Visit Upcoming Courses
Folder: About
Back
About Hide Tanning
Hide Tanning Resources
Hide Tanning Tips
Fern + Roe FAQs
Folder: Learn With Us
Back
Courses we offer
Upcoming In-person Courses
Private Group Instruction
Hide Club
Self-paced online courses
1:1 Mentorship
Hide Club: SUMMER CAMP
Shop For Tools
Visit Upcoming Courses
Shop Alum + Salt
2.png Image 1 of
2.png
2.png

Alum + Salt

$13.99

Alum is used as a mordant in natural dyeing and as a tawing agent in hide tanning. It preserves hides, helps secure the hair in fur-on rugs, and acidifies (which has a natural preservative effect). Alum is used in mineral tanning combined with oils and as a base for smoke-tanning and bark-tanning.

This product is equal parts alum and salt (sodium). It is 4 cups total; about 4 pounds.

Directions:

Use the entire contents of bag for a large fur-on hide such as sheep or deer.

Use 1/2 cup of alum-salt for making chamois (cloth).

Use 8 cups total of an alum-salt mix for large hides such as bear.

After de-salting or thawing a hide, rub this mixture on the skin side with gloved hands.

Place the hide in 8-10 gallons of water.

Let sit for 5-7 days.

Quantity:
Add To Cart

Alum is used as a mordant in natural dyeing and as a tawing agent in hide tanning. It preserves hides, helps secure the hair in fur-on rugs, and acidifies (which has a natural preservative effect). Alum is used in mineral tanning combined with oils and as a base for smoke-tanning and bark-tanning.

This product is equal parts alum and salt (sodium). It is 4 cups total; about 4 pounds.

Directions:

Use the entire contents of bag for a large fur-on hide such as sheep or deer.

Use 1/2 cup of alum-salt for making chamois (cloth).

Use 8 cups total of an alum-salt mix for large hides such as bear.

After de-salting or thawing a hide, rub this mixture on the skin side with gloved hands.

Place the hide in 8-10 gallons of water.

Let sit for 5-7 days.

Alum is used as a mordant in natural dyeing and as a tawing agent in hide tanning. It preserves hides, helps secure the hair in fur-on rugs, and acidifies (which has a natural preservative effect). Alum is used in mineral tanning combined with oils and as a base for smoke-tanning and bark-tanning.

This product is equal parts alum and salt (sodium). It is 4 cups total; about 4 pounds.

Directions:

Use the entire contents of bag for a large fur-on hide such as sheep or deer.

Use 1/2 cup of alum-salt for making chamois (cloth).

Use 8 cups total of an alum-salt mix for large hides such as bear.

After de-salting or thawing a hide, rub this mixture on the skin side with gloved hands.

Place the hide in 8-10 gallons of water.

Let sit for 5-7 days.

You Might Also Like

IMG_3935.jpg IMG_3935.jpg IMG_3935.jpg
Wool Comb
$14.99
Mezzaluna IMG_3943.jpg IMG_3944.jpg IMG_3945.jpg
Mezzaluna
$29.99
Salted Sheep Skin Set Sheepskin rug made naturally, plush wool.png 20220801-0A4A7070.jpg
Salted Sheep Skin Set
$69.00
Waterproof Apron Screen Shot 2021-11-26 at 2.18.27 PM.png
Waterproof Apron
$24.99
Gift Certificate.png
Gift Certificate
from $25.00
Logo_small.png

About

About Us

About Hide Tanning

About Mara Cur

FAQ

Contact Us

Terms Of Service

Resources

Learn With Us

Custom Instruction

Upcoming In-Person Courses

Hide Club


©Fern + Roe 2021